Does ASTM spec SB-862-2 have a P number ?
By
dlmann
Date
11-07-2007 15:35
Hello Joe:
If your SB-862-2 is the same as SB-862 grade 2 then P No. 51.
Regards, Donnie Mann
By
InspectorJoe
Date
11-07-2007 16:00
To Donnie Mann:
Thanks,
Joe D.
Topic
Welding Industry
/
General Welding Discussion
/ P Number
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill