- - By dan 14 (*) Date 12-27-2007 16:22
why does it seem that lincoln excalibur 7018 runs so good but the 7018-1 runs wet and rough?  is there a certin tecnique i should be using?  hobart 7018-1 runs great but i can't always get it
Parent - - By Justin O (**) Date 12-28-2007 03:30
What are you welding on?
Parent - By dan 14 (*) Date 12-28-2007 17:54
mostly pipe.  the qc manager has elected to use only 7018-1.
Parent - By raftergwelding (*****) Date 12-29-2007 00:40
turn down the heat
Parent - By JescoPressure (**) Date 12-30-2007 06:09
throw them at the qc? Do you guys in the states ever run liquid air 7018 down there? It's pretty much the standard up here in Canada for the most part.