HI, I have a bobcat 225 and put my @ 85 amps, with 1/8 5p+, went the fit-up is 3/32 land and 3/32 root and on big pipe 90 to 95 amps on 1/8 land and 1/8 root, put the amps setting @ 70-150 and the fine ajustment work it betwing 3 and 4, i'll hope this help you.