/ RETESTING OF FAILED WELDER
By
MOHAMMED KAMEL
Date
07-30-2001 11:18
IF A WELDER HAD FAILED TO PASS A TEST , WHAT IS THE MINIMUM TIME AFTER WHICH HE CAN BE RETESTED.
By
kpauley
Date
07-30-2001 11:46
AWS D1.1-2000 Section 4.32 should give you all the info you need.
By
GRoberts
Date
07-30-2001 14:33
ASME Section IX says that a welder can be retested immediately, but he has to pass essentially 2 tests. He can retake the test (only one test) after further "practice" or "instruction". The code leaves the amount of either up to the certifier.
Topic
Welding Industry
/
Technical Discussions
/ RETESTING OF FAILED WELDER
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill