- - By Richman (**) Date 07-23-2008 11:10
[deleted]
Parent - - By Jim Hughes (***) Date 07-23-2008 12:09
Richman,
Look at the PFI (Pipe Fabrication Institute) they have some guidelines. Also, if it is ASME then B31.1 gives you some guidence.

Thanks
Jim
Parent - - By jon20013 (*****) Date 07-23-2008 12:25
Good answer, Jim.  I was going to say this is "normally" project spec stuff but both sources you mention are good guidance.
Parent - By js55 (*****) Date 07-23-2008 19:53
PFI ES-3 to be specific.