Welding Industry
/
Technical Discussions
/ 5Cr 1/2 Mo
By
krishnan sivaraman
Date
08-12-2008 09:01
Can anyone provide me literatures on welding of 5Cr 1/2 Mo material.
By
tom cooper
Date
08-12-2008 15:40
Edited
08-12-2008 15:43
look in ASM Handbook, Volume 6. Then look for ASTM A387 Gr 5 data.
Also look in the Kobelco Welding Hanbook (pdf online) and use the search tool for "5Cr-0.5Mo"
They will both give you fillers, preheats, post heats, etc.
By
sunil mani
Date
09-07-2008 13:07
Yes, 387 Gr 5 is standard specification for pr.vessel plate.But if you are dealing with piping ,then you have to search ASTM A335 grouping.
By
sunil mani
Date
09-07-2008 13:10
From my exp. for root pass welding u can use ER80S-B6.For filling and capping u can use E8015-B6.
Topic
Welding Industry
/
Technical Discussions
/ 5Cr 1/2 Mo
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill