Cumminsguy71 -
If a welder qualifies to a 6G test, they are also qualified to weld in the Flat, Horizontal, Vertical, and Overhead positions.
And I believe using a 7018 which is an F4 designation, will also allow the welder to use 6010 which is and F3 designation.