- - By bozaktwo1 (***) Date 10-06-2008 20:04
I have an old drawing that calls out a finish QQ-P-416, Type 2 Class A.  The problem is, the latest revision of QQ-P-416 (F) (Cancelled) calls out classes in number format, not letters. 

Does anyone have an old (c. 1954) copy of this specification?  Or does anyone know where I can cross-reference the plating thickness class?
Parent - By bozaktwo1 (***) Date 10-18-2008 13:01
I'll update this for y'all...since no answers were forthcoming, my engineer and I explored the latest copy of the spec (keep in mind this spec was cancelled and not replaced in the 90s), and came up with class 1 for plating thickness of .00050" min.  After discussing the requirement with the drawing's owners, it would appear that there was once a lazy detailer out there in aerospace land...:)
Up Topic Welding Industry / Welding Fundamentals / Plating Specs

Powered by mwForum 2.29.2 © 1999-2013 Markus Wichitill