Hi I'm new to the welding industry.Can anyone pls tell me What is meant by the letter "G" which appears in 2G, 3G, 4G etc?
By
jrw159
Date
10-30-2008 14:49
Nandesh,
This refers to they type of weld. G is groove and the numbers represent the potition of the groove. Here are some attachments that explain it fairly well. Hope these help.
jrw159
Attachment:
wc473.pdf
(382k)
Attachment:
wc474.pdf
(438k)
Attachment:
wc475.pdf
(532k)
Attachment:
wc482.pdf
(418k)
By
Nandesh Kumar
Date
10-30-2008 15:27
Thanks a lot Mr.jrw159
By
jrw159
Date
10-30-2008 15:29
Anytime. :-)
Topic
Welding Industry
/
Technical Discussions
/ what is G?
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill