Does AWS D1.1 have a table for testing criteria that must be met for this type of structure or does the EOR need to specify the criteria?
By
hogan
Date
12-09-2008 18:09
if your speaking of NDT then AWS does not mandate anything for production welds other than visual.
By
contractor
Date
12-09-2008 20:14
Maybe I am mistaken but I thought cyclically loaded CJP welds needed to be UT or RT tested.
By
hogan
Date
12-09-2008 20:54
I could be mistaken. Do you have a code reference?
By
ctacker
Date
12-09-2008 22:11
He may be refering to clause 6.11.1 (2008)
By
contractor
Date
12-10-2008 11:49
I am referring to 6.13.3.
By
contractor
Date
12-10-2008 13:37
Also it is tubular.
By
pax23
Date
12-10-2008 16:56
Have you seen the new commentary C-6.11.1 on this issue. It may help you. It is new to the 2008 edition. Page 484.
Topic
American Welding Society Services
/
Technical Standards & Publications
/ Cyclically Loaded Tubular Structure
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill