Up Topic Welding Industry / Inspection & Qualification / Min reinforcement for butt [CJP] joints
- - By hburg rocket (*) Date 09-02-2009 21:58
I know that the max reinf is 1/8" [per D1.1 para 5.24.4 and Fig 5.4 (D)], and that there is an "unacceptable" underfill.  Is there a min reinf for butt joints? 

For unequal plates, can the reinf = "0" , i.e. be "staight" between the two plates?

h'burg rocket
Parent - - By HgTX (***) Date 09-02-2009 23:43
There is no minimum reinforcement; it can be completely flush.  I don't see how you'd get there without underfill unless you welded with *some* reinforcement and then ground it flush, though.

The way I read 2.7.1 and 2.16.1.1, yes, it can be straight between the plates as long as the slope is no more than 1:2.5.

Hg
Parent - By hburg rocket (*) Date 09-03-2009 14:43
Hg, thanks for your input!

That is what happened - they ground it flush afterwards.

hburg rocket