- - By tigrooter (**) Date 09-23-2009 19:49
Has anybody used sawyer mfg bevelers. I've only used h&m and m&d. They look okay just never used one.
Parent - - By TRC (***) Date 09-23-2009 23:19
Yes, they are as good as anyone else. I've used the bands up to 36" and the saddles- Ted
Parent - - By Robert48 (**) Date 10-02-2009 02:36
I just got off a pipe piling job where I used a H&M band type in the horizontal position (pipe stucking out of the ground). This was a pain in the as$. It was almost a three man job to set up. One to hold the machine, one to hold the chain, and one to attach the chain together and tighten it up. Would these be easier to set up and deliver the same quality cut? They look smaller and I did not see a chain on pics in the link below.
Parent - By RUSSELL (**) Date 10-03-2009 01:59
they are lighter and easier to set up by yourself in this type of situation than H&M's or MATHEY's.The smallest one has a locking bar with set screw,and the other 2 sizes have chain & boomer.
Parent - - By cmays (***) Date 09-24-2009 01:23
They have a web site?
Parent - By RUSSELL (**) Date 09-24-2009 04:19
I got 3 different Sawyers & I like'em.Easy to change size of pipe,no spacers(dawgs) to lose,easy & quick to set up,&more sizes of pipe to 1 machine.I got the 1.5"-4",3"-8",8"-14".
Parent - - By weldwade (***) Date 09-24-2009 22:56
http://www.sawyermfg.com/

Never used one but here is the website.
Parent - - By up-ten (***) Date 09-25-2009 01:45
Thanks for the website. Checked it out and I'm fairly impressed, no spacers to keep track of and it gives you a nice square cut every time. Now they just gotta sell 'em up here and I'll hang one in the truck for sure.
Parent - By raftergwelding (*****) Date 09-25-2009 07:08 Edited 09-25-2009 07:50
heres an idea how much you looking to spend i bet i could find 1
Parent - - By paul prill (*) Date 09-25-2009 11:46
Here is the tough weld web site, they are a branch of Sawyer, i have bought a lot of stuff from them with very good results. www.toughweld.com
hope this helps.
Parent - - By up-ten (***) Date 09-25-2009 14:30
Thanks Shad and Paul,I've got the toughweld site bookmarked. I think my old mathey fell off the deck one too many times and it hasn't cut square since unless thats an inherent characteristic of mathey bevellers.
Parent - - By RUSSELL (**) Date 09-30-2009 15:09
welders&equipment in Alexandria,LA talk to Don Miller #(318)443-6386.He can get you a SAWYER for as cheap as he can.
Parent - By RUSSELL (**) Date 10-01-2009 16:21
For anybody in Ks. or OKL. LAMPTON WELD SUPPLY did carry them.
Parent - - By up-ten (***) Date 10-03-2009 02:58
Thanks Russell.
Parent - By RUSSELL (**) Date 10-03-2009 04:12
Anytime I can help I sure try.That is what we are here to do,help each other as best we can.