- - By JeremyW83 (***) Date 12-19-2009 01:58
I got a free 10* can of 1/8 LowHigh Downhill Lincoln.  I am wondering what amperage range to start out at for trying them out.
Parent - - By Cactusthewelder (*****) Date 12-19-2009 02:20
Not sure. The lincoln website may have a range for you, I would start around 125 amps and go from there
Parent - - By JeremyW83 (***) Date 12-19-2009 02:40
Thanks Cactus.

I got em free from an Airgas.  Somebody had them order them and never showed back up.  He just handed them to me and said to try em out.  I figure I should probably try and get my hands on some 12" to try it out on.
Parent - - By downhandonly (***) Date 12-20-2009 01:58
try 3rd gear and 70 downhill lohi has gotta be smokin :)
Parent - By okwelder82 (***) Date 12-24-2009 23:30
I agree with downhand it has got to be HOT or it didnt seem to run right for me.