- - By Firefly (*) Date 04-01-2010 22:41
Dear All,

My 1st post!!!

Thank you for a great forum.  I have found many answers here.

My question: I have heard the term "Intermediate Stress Relief".  Could anyone explain what the purpose of it is and when it should be applied.

Rgds
Cedric
Parent - - By js55 (*****) Date 04-02-2010 12:28
I guess my mind is a blank right now on intermediate stress relief. Intermediate post weld heat treatment is a long hand way of saying hydrogen bakeout.