If you can, you should check with the designer/engineer to see what the intent is.
That joint detail is often used where a fillet might be specified, but it becomes a groove configuration because of the plate angle.
You really don't want to backgouge that root if you don't have to - so it might be that partial joint penetration was actually intended but not shown.