mike wiebe 3
Date
08-13-2010 15:54
Anybody know if inconel 625 weld wire will be combatible to use on inconel 601? First place was here to start my search, thanks.
By
MMyers
Date
08-13-2010 16:20
625 is not listed in the data sheet as a recommended consumable. Recommended consumables are dependent on application and welding process. See page 14 of the data sheet:
http://www.specialmetals.com/documents/Inconel%20alloy%20601.pdf
By
mike wiebe 3
Date
08-13-2010 16:37
Excellent site! Thanks again.
Topic
Welding Industry
/
General Welding Discussion
/ Inconel 601
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill