- - By Zeek (**) Date 03-10-2011 17:27
Is there anything in D17.1 that specifically requires you to use GTAW?  Is it permissible to use GMAW with this spec?
Parent - By Ringo (***) Date 03-10-2011 17:38
yes,its listed in section 5.
Parent - - By Lawrence (*****) Date 03-10-2011 18:00
Zeek,

The *fusion* welding processes are listed in D17 Table 5.1

Please keep in mind the Procedure (PQR/WPS/Welder Performance) qualification requirements that go along with a change in process.  See 5.2.2.1
Parent - By Zeek (**) Date 03-15-2011 18:13
Thanks.  I completely missed it...it was in Table 4.1