/ PWHT hardness limit per ASME VIII
By
carlos_correia
Date
04-01-2011 14:37
Does ASME Sec.VIII Div. 1 specify some limit hardness values for materials after PWHT (as NACE MR0175)?
By
jrupert
Date
04-01-2011 20:34
The only section that requires it is section UF-31 specifically for liquid quenched and tempered SA-372 forged material. Unless you have this specific application, then no hardness testing is required after PWHT for any other material.
By
carlos_correia
Date
04-08-2011 04:42
Thank you !
Deeply appreciated !
By
G.S.Crisi
Date
04-08-2011 17:03
Carlos,
a curious question: is it that NACE standard related to deaerators design and fabrication?
Giovanni S.Crisi
Sao Paulo - Brazil
Topic
Welding Industry
/
Technical Discussions
/ PWHT hardness limit per ASME VIII
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill