Not logged inAmerican Welding Society Forum
Forum AWS Website Help Search Login
Up Topic Welding Industry / Technical Discussions / Welding Aircraft Tubing
- - By Don Hansen Date 12-01-2002 18:53
I've seen several references to TIG welding 4130 aircraft tubing with either ER70S-2 or ER70S-6. What are the differences in these two filler rods. Is one preferred over the other for welding 4130? and if so why?
Don Hansen
Parent - By airweld (**) Date 12-01-2002 21:46
http://home.hiwaay.net/~langford/sportair/
http://www.tigdepot.com/

You will find info on TIG welding airframe tubing at these sites. Good luck, Scott.
Parent - By TiG6al-4v (*) Date 09-12-2003 03:05
ER80S-D2
Up Topic Welding Industry / Technical Discussions / Welding Aircraft Tubing