- - By KennyCalJr (*) Date 03-15-2012 20:33
A quick question for you guys:

do u think these settings are good for the material I work on?

Mig Welding
Wire size: 0.35
Amps: 126
Wire Feed: 200
75% 25%
Arc Control: 90
Machine is a Miller XMT 200 and a Miller S-22
Material Company uses to build Awinnigs is 18 Gauge

Thank You
Parent - - By 357max (***) Date 03-15-2012 21:40
Voltage about 17 ~ 18. Gas flow rate 20 CFH. What is the wire stickout past the contact tip/tube? ~ About 1/4 ~ 3/8 & using a push gun travel angle. I believe the arc control is inductance control I would set it at 50% or lower. Lower if the starts are "stumblying" higher if spatter is an issue.
Parent - By KennyCalJr (*) Date 03-15-2012 23:56
Thank You, I will try it tommorow and see what happens.