- - By Jonesy15 Date 01-28-2013 04:36
Was wondering if anyone could help me out. I was wondering the difference between NR-211-MP E71T-11 and NR-305 E70T-6 are, or at least where to find the information. and thoughts are much appreciated.
Parent - By Shane Feder (****) Date 01-28-2013 08:45
Jonesy,
Try this
http://www.lincolnelectric.com/en-us/consumables/flux-cored-wires-self-shielded/Pages/flux-cored-wires-self-shielded.aspx

Your E70 is in the "Flat & Horizontal" section and your E71 is in the "All Position" so there is your first answer as to differences.
Hope that helps,
Cheers,
Shane
Parent - By Jonesy15 Date 01-28-2013 17:56
thanks every bit of info helps.
Up Topic Welding Industry / General Welding Discussion / Differences in electrodes.