- - By lany luna Date 12-11-2013 11:19
does anyone have ever do the job  on "magnesium alloy brazing",or does any one know any institute who are expert on brazing,please recommend some?  thanks alot and have a great day.
Parent - - By lany luna Date 12-12-2013 07:57
IS there anyone can give me some information?
Parent - By SCOTTN (***) Date 12-12-2013 12:43
This link may help.  Scroll down to 9.2:

http://www.intechopen.com/download/get/type/pdfs/id/12757

Also, if you have access to Volume 4, Seventh Edition of the Welding Handbook, published by the AWS, there's information on brazing magnesium alloys.... pre-braze cleaning, furnace brazing, torch brazing, dip brazing, and post-braze cleaning.