6 x 1/4"" 420 flat bar to 12" sch 80 309 ss
a fillet weld on to the pipe
butter the 420 end with 309 filler and then weld together with 309?
no code, but use asme, for baseline
on the right track?
thank you for your time and consideration
sincerely,
Kent
edit: gmaw for the buttering and smaw for the fillet
'