- - By Nalla (***) Date 01-28-2017 20:24
Dear Sirs
Base Material - API 5L X52
Test Position - 6GR- Fig 9.26
Weld Process- GTAW + FCAW  &  GTAW +GMAW ( 2 test Coupons )

When PQR Qualification performed in conformance with Fig 9.26 and Table 9.8 & 9.9, Does Mock Test required as mentioned in 9.15.4.1?
My understanding - Not Required

If required, please explain
Parent - By Nalla (***) Date 02-23-2017 13:52
Dear Experts
Pls enlighten me if my understanding is correct