FYI  just did  side bend test on A514 1" plate ,1/16" root opening no backing( CJP) , GTAW root pass( ER70S-2),fill and cover with ER7018 H4R , Also used a 2" ram (instead of the 2 1/2" one) IT CAME OUT FLAWLESS  Had a liitle time to spare today lol!!! also this is the first time on the original forum that I have heard so much about from BRENT ON THE NEW FORUM . I TO LIKE THIS FORUM . IT IS EASY TO USE AND FIND ALL THE GOOD STUFF QUICKLY MUCH BETTERRRR !! THANKS BRENT AND TO ALL OF YOU GUYS!!!
Parent - By jwright650 (*****) Date 11-30-2017 11:51
Congrats, bending with the tighter radius is an accomplishment.
I like this forum better too. I like simple and easy when I'm busy...this forum is simple and easy.
Parent - By Tyrone (***) Date 11-30-2017 13:32
Excellent irontaint and welcome to the original AWS Forum.
- By irontaint11 Date 11-30-2017 13:54
just aliitle experiment on under matching filler topic
Up Topic Welding Industry / General Welding Discussion / Bend test A514

Powered by mwForum 2.29.2 © 1999-2013 Markus Wichitill