- By Rajasekaran.V Date 02-12-2018 10:41
I am rajasekaran from india,we are tig welding 1mm ss304 grade material.
We are welding in fusion method.
Steps we are following are :
Blanking , forming, grinding two half's manually , tag welding in tig , finally automatic tig welding with research grade gas.
While welding we are facing some areas unweld .

Pls suggest were we are not correct.
- - By Rajasekaran.V Date 02-12-2018 10:42
Regarding my quary , i am collecting some photos ..i will be sending it soon
Parent - By TerryTerzian (*) Date 02-12-2018 19:50
Welcome.

In addition to photos, how about a list of parameters?
Up Topic Welding Industry / General Welding Discussion / Tig welding ss304 1mm thick