Up Topic American Welding Society Services / Certifications / RT replace for Bend testing in Table 11 in AWS CWI part B
- - By vuong01c1 Date 06-14-2018 07:43
Dear colleagues,

I am going to take exam for AWS CWI in next few months but there is one point in table 11 of document AWS CWI practical BOS: 2017 make me confuse.

Table 11 quotes that: "Radiography may be substituted for bend testing for the SMAW, GTAW, GMAW (except short-circuiting), and FCAW processes, as
applicable, for qualifications".

As my standpoint, examination requirements for performance qualification are: Visual examination + RT. Bend testing is optional If welder uses SMAW, GTAW, GMAW and FCAW (because RT may replace for Bend testing).
When performance qualification uses GMAW (short-circuiting) process, examination requirements are (mandatory): Visual + RT + Bend testing

Please help me to clarify. Many thanks for your clarification.
Parent - - By Steelslinger (**) Date 06-14-2018 12:40
It is easier to look at it as:

Visual + Bend Test or RT - for SMAW, GTAW, GMAW (except short-circuit) and FCAW

Visual + Bend Test - for GMAW-S (short-circuit)
Parent - By vuong01c1 Date 06-20-2018 07:44
Many thanks, bro.
Parent - - By welderbrent (*****) Date 06-14-2018 14:34
DO NOT PAY ANY ATTENTION TO ANYTHING YOU THINK YOU KNOW WHEN IT COMES TO THE PART B BOOK OF SPECIFICATION!! 

Yes, I did put that in all caps on purpose. 

Whatever your normal code is, it does not apply here.  And, l don't know what you are referring to, according to D1.1 Clause 4.16 VT+ bend tests are required BUT RT may be substituted.  Thus, it is worded like the BOS. 

Memory is a bad thing during the Part B.  Don't even think about your job and the applicable code you normally go by nor your shop/work QC manual.  It will mess you up.  Just read it (BOS) at face value and go with what it says.  

He Is In Control, Have a Great Day,  Brent
Parent - - By vuong01c1 Date 06-20-2018 07:44
Thank you very much, Mr. Brent
Parent - By 803056 (*****) Date 06-23-2018 01:18
Brent hit the nail on the head.