- - By Bryan Bidewell (*) Date 11-17-2023 10:53
I understand the requirements of Fillet Weld testing in accordance with Figure 6.15 of AWSD1.1 (Fillet Weld Soundness Tests for WPS Qualification.  What I'm struggling with is, if I produce a test piece with a single fillet one side and a multipass fillet the other side, can they both be included in the one PQR, to qualify a single pass WPS and a multipass WPS?

Thanks
Bryan
Parent - By Lawrence (*****) Date 11-17-2023 13:09
See 6.13.2

You are cheap   :)

Lol