Can anyone refresh my memory on how to calculate the heat input to a welded joint? Thanks.
Parent - By R. Johnson (**) Date 10-09-2000 14:21
Joules/inch = (amps x voltage x 60)/travel speed in inches per minute
Parent - By MBSims (****) Date 10-10-2000 02:14
Mr. Johnson's formula works especially well for tall, long-legged ex-Navy nuke welders.