Thanks Chuck, we'll try that too,. Another question in terms of shielding. I have read one recomendation from Hastelloy that contrary to common practice, it is recommended that the purge pressure be somewhere in the range of 4X the torch presure, torch pressure being reduced to about 10 cfh. What are your thoughts on that?