By MattR
Date 09-01-2005 17:26
Thanks guys! It sounds like no matter what I'll have atleast a little bit of weld prep to do. No biggie, but I do want to keep it down to a minimum.
I would still like to know what gas is needed (if other than shop air) for plasma. The reason is that the shop that would cut the parts if I choose plasma, is not exactly keeping up with technology, so I'd like to make sure they use the correct gas. Beyond that, they're great.
Bill, I do have access to a water jet, just checking out options at this point. I am alittle concerned with rust as the parts will be shipped.
(Edit: Pushed the wrong "Reply" button, sorry guys.)