Addenda Issued for D1.9, Structural Welding Code — Titanium The following addenda has been made and incorporated into the current edition of this document. AWS Standard: D1.9/D1.9M:2007, Structural Welding Code — Titanium Addenda No.: ADD1 Subject: Radiographic Crack Allowance in Table 5.2 Page 81: Add a row above “Fine Scattered Porosity” to Table 5.2 for cracks discontinuity types as follows: Inspection Trends / Fall 2011 31