>I had forgotten about 5.26
How about 5.30 Weld Cleaning, 5.30.1 In-Process Cleaning, and 5.30.2 Cleaning of Completed Welds?
5.30.1 In-process cleaning.
Before welding over previously deposited metal, all slag shall be removed and the weld and adjacent base metal shall be cleaned by brushing or other suitable means. This requirement shall apply not only to successive layers but also to successive beads and to the crater area when welding is resumed after any interruption. <snip>
5.30.2 Cleaning of completed welds
Slag shall be removed from all completed welds, and the weld and adjacent base metal shall be cleaned by brushing or other suitable means. Tightly adherent spatter remaining after the cleaning operation is acceptable, unless its removal is required for the purpose of NDT. Welded joints shall not be painted until after the welding has been completed and the weld accepted.
EDIT*...I should read better, Lawrence has already covered these points.