![](/mwf/attachments//avatars/4269-2369.jpg)
I was wondering the correct procedure to go back and fix an error I have on some WQR's that I have done in the past. Computers are great tools when in the right hands, but this dummie (ME) had an error on my original template that has been duplicated to several WQR's before I caught the error. The error is concerning the bend test and it's acceptability. I had copied a template that I was using for 1" plate B-U4a groove qualifications and then I was changing the info so I could qualify on 3/8" plate in the same positions and processes, etc. Where I made my mistake was in the bend tests, I did not change the info to read "root and face" bends, it still has the 2 "side bends" listed. What would you guys suggest I do to correct these documents correctly. I don't need some inspector calling my hand on these.
HELP PLEASE,
John Wright