It's tough. you get info from as many people as you can. you go to sites but, here's the thing. you can travel 350 500 or more miles to job site. don't mean you pass the weld test and get job.
CWI's are ruthless
your to slow
your to fast
your late 4 mins no test etc... one time I didn't even get to test just the way I looked was enough. haha
hotel could be 50 miles from job site
Jomax was my last ditch effort for pipeline work for awhile. when I failed that test two weeks ago. after driving 350 miles to and 350 back and hotel for a night. I came home. got 35 bucks an hour close to home (4 miles)no per diem but lots of work and OT
plus I still fab my remote boxes and make extra money. I'm happy for the moment and my business gets to grow.
if you ain't tried pipeline work stick to single hand. 32 from JV ain't bad and per diem too.