The job is going as planned. It is taking a little longer than originaly planned to get all of the drawings approved. But, I think they will be aproved to order steel on July 10. This should put us starting fabrication the first week in August. THE PAY WILL BE $55.00 PER HOUR FOR WELDERS. I also need Structural fitters with RIG experience. Pay BOE. We will be working all the hours you can stand. We are still working on pay days. The will be at least every two weeks. I am trying to make it every week. Test will be either 1/2" or 1" vertical plate.As per the Engineer ,all rods used will be 70XX. No 60XX allowed. (so dont get caught) THIS IS AN A.P.I. job All welders, steel and rods will have certs. For those of you who dont know, When you buy rods ask for the certs on the batch. They will know what you mean. KEEP THE PAPERS THEY GIVE YOU! YOU WILL NEED THEM. I am trying to buy rods at a pallet price so everyone will get a break on rods. All supplies are the same, I am working on getting all of us cheaper prices. I still need welders so once again, If you are interested and you have not sent me an Email. PLEASE DO SO at djmeroney@hotmail.com Fitters do the same. I will post the location and a contact phone # within a week or so. Know this, I AM A RIG WELDER. I have been for 28 years. I am trying to get this job set up the way we all wish they all where. However I am not perfect so when we get there, if you see something we can do better, let me know I'll do my best. We have 12 rigs to build on the first order. The first one will be built alone so we can work out the bugs. Then we will build 3 at a time.
Thanks
Cactus
Cactus,
It sounds like you have a pretty good plan coming together. Just out of curiosity, who is doing the inspection?
jrw159
We have a IN HOUSE CWI as well as API inspectors
Cool, if you need help let me know. I have a referance for an inspection position if you find the need.
jrw159
Cactus-\
I have a couple of guys I'd like to forward the info to. PM me with your contact info.
K
How long do you think this job will last?
This job could last several years. Its hard to tell. Most of the Rigs are going overseas so as long as they have money we will build rigs. They are paying 50% in advance so there is alot of money on the line. Like I said, the first order is for 12 rigs
The yard is in central West Texas. I will post the exact location sometime this next week. The company has ask me not to give exact details on location until plans are finalized. I understand their reasoning. Thay are trying to avoid 200 phone calls per day and Welders driving up with inquiring minds. I will list it a.s.a.p.
Hello Cactus, Hey I have a bang up fitter. We're working in Lake Whitney right now but we will be ready when this kicks off.
Can you give me any info on what thier willing to pay for fitters.
Bob
Hey cactus, you should be recieving my e-mail soon. I just e-mailed you my contact info for this job.
Ill look for it. I will contact everyone who sends an email as soon as I can start hiring
Oh , is there going to be any per diem? Just asking...
no per deim I dont know of ANY yards in texas that pay it. I guess they figure a long term job that you can count on EVERY day is per deim in itself
Do you know more or less the exact location in central west tx??
Yes I do know more or less where the exact location is. I will release that info as soon as I can. Trust me, I am as ready as anyone to get this started. I wish it started last month. But I am trying to follow the rules and do what has been ask of me so I dont mess it up for everyone. This company has used Rig welders in the past and from what I am told, they where takin for a ride. I am doing my best to overcome what someone else did. Its not easy. But I'm getting it done. So, Once again, I truly hope to be able to release this info by Friday. I have a meeting again on Thursday to iron out some final details and order steel.
Cactus i have a friend that is a rig welder also and if you would can you call him also and his name is fred and his number is 832 283 9470
Rick I am going to the site in my truck tommorow to look for rv parks. It is the first time I have been there without an airplane. I will post RV parks Friday night as I find them
What is a finish fitter ? I always thought you can fit or you cant fit.
I thought that rig for Parker was supposed to last over a year ?
Hey cactus, you get the lo down on that job? You never posted the info since your meeting on Thursday. Is it still on?
It is still on. Our target start date is Aug 4. The rigs will be built in Brady Tx. I will be contacting people next week. The steel has been ordered and our final plans will be issue to us next week. The welding test will be a 1/2 plate vertical with backer strap also a 1/2 plate 6010 root 7018 fill and cap and 6" 6g 6010 root 7018 fill and cap. The open root plate and the 6g will be for guys welding on the derrick. Also, the only cell phone service that seems to work here is AT&T. The subs will be fit together and tacked with 7018 then rolled and welded out with 7024 or 7018. Specs call for al 70xx rods unless on derrick Derrick is all 6010 root and 7018 fill and cap. This is an API shop. so all rods will be kept in ovens. I will get some community ovens but I am going to buy my own 50lbs rod oven to keep on my truck. I know the honor system should work, but it doesnt always. I just prefer to know I am the only one using the rods I pay for. The 50 lb ovens only cost about 200 bucks so i figure its a good investment. Also This company WILL DRUG TEST. As soon as I get a phone that works in this area I will post my number for contact. I should get a Phone by tommorrow and internet that works all the time. I will get the local welding supplies listed asap so everyone can open accounts that need to. I am working on getting us all special pricing. There is not much going on here work wise so the welding supplies are eager for business. But overall its all going as planned now
Sure wish i still had a moble welding rig.. just got let go where I work.
Do the welders need to pass both plate and pipe test to weld or will they be welders only doing plate?
Gary
The root is downhill 6010 for the Derrick test. The test with a backer strap will be uphill 7018 all the way. Not everyone will be tested for Derricks. Once we finish the welds on the sub and derrick they will be Mag Particle tested
what size of rod is being used?
test with 1/8 but we will be running 1/8-7/32
Will the pay be the same for everyone, or will it differ as to the job..... Derrick Welders vs. Substructure?
what will be the pay for fitters and do fitters have to test. do you no how far to the nearest camp ground or rv park
is the root uphill or downhill?
please e-mail me, my name is Austin Duncan. Duncancustomwelding@yahoo.com or call me 918-285-0205 would like to talk more with you. In from Stillwater ok but working in rifle co. I could bring at least 5 good hands.
hey cactus, does it still look like aug 4th start date. if so would we start testing on that monday the 4th then go to work the fifth or how are you gonna run that. just wondering because i am gonna be on a job for the next two weeks then i am planning on coming to brady to work with you. my last day should be on the 2nd but if i need to be there earlier than the fourth i can make arrangements. also i have emailed you with my contact info. thank you
Yes we will test on Monday the fourth. I will call those who are going to test on the fourth. Then I will test more the following week
the ones that test on the 4th will they start work on the 5th
they will start on the fourth if they pass
are you gonna do half the first week then half the second
The test will only take a couple of hours
are they gonna bend test two coupons from your test plate
Yes we will bend them and I am testing 15 on the fourth
are you testing the first 15 that emailed you first
If you are chosen to test on the fourth you will be called
are you getting maxed out on the number of welders you need
No Im not I will have probably 80+ by October
thanks for the info, i am ready to come down as soon as you call. it has been slim pickens around here so i am excited about this new opportunity
it will be nice to get out of oklahoma for awhile
a friend of mine worked in brady for a week last year and he said it is a very nice community friendly people with an outstanding barbecue joint
I would like to test! 1 870-278-3605