There are copper filler metals available for welding copper.
Whats the application..Are these electrical contact bars?
Is your base metal pure copper, or some bronze alloy like copper-zinc alloy, or maybe a copper-tin alloy, copper-aluminum, copper-nickle, etc.
A 40% silver filler material sounds more like a brazing than a welding mat'l.