I thought the code required all 12 inch and over to be welded with two welders. One good reason is that the joint gap will close up if you use just one welder.
done it plenty of times especially on heavywall. I'm a tube welder we brother-in-law everything just about, ofcourse we have to since you can't get to the other side from inside a boiler.