- - By up-ten (***) Date 09-10-2008 10:01
I've often heard one of these terms used but never a definitive answer. What is this weave really describing? Is it an uphand cap or a downhand cap?
Parent - By Cactusthewelder (*****) Date 09-10-2008 14:08
IT IS A TERM FOR A 7018 UPHILL CAP PASS. IT IS NOT USED MUCH ANYMORE IN PIPE BUT YOU STILL SEE IT ALOT IN STRUCTURAL WELDING AND IN THE OILFIELD
Parent - - By hogan (****) Date 09-10-2008 14:32
Here is a previous post on the topic, hope it helps.

http://www.aws.org/cgi-bin/mwf/topic_show.pl?pid=81207;hl=texas%20weave
Parent - - By up-ten (***) Date 09-10-2008 15:36
Right on!! Thanks for the direction on that. I'm guessin' some guys here  where I am, use that term quite liberally and it just became unclear from one guys description to the next.
Parent - By hogan (****) Date 09-10-2008 16:09
The search function for this forum has been very useful for digging up information.