Hi all...I am trying to weld SS 304 using 98Ar-2CO2 and Fronius 2700 power source. Spool is 308. I tried a lot to set the pulse parameters, but not able to get a desired quality of weld. I searched the whole manual as well as internet to get parameters, but failed again. Can anyone suggest me the best parameters for this kind of welding in the thickness range of 1.5 mm with 1.5 mm sheet, fillet welds? Any literature to learn in depth about pulsing also would be a great help later on.