All I can tell ya is take a gap bigger than your filler wire. Feed your wire from the inside. Doing this, coming off the bottom to the side, you shouldn't have any suck back. Instead, you should have a bead with some meat. Then when you come off 10 and 2 o'clock poistion, just lay the wire in the bevel and run over the wire. The bead will just fall in there.