So what were you doing when the axles broke? btw sounds like they may have been improperly heat treated.
A friend of Mine got a 700 Polaris in '03, had a lot of grief from it.
Ask Polaris who made the axles, what they are made out of & where they were made or you'll get a lawyer to find out and I bet they make a deal with you! Had 3 Polaris 4 wheelers and never had any kind of problems like you had.
By tigrooter
Date 03-26-2009 07:07
Edited 03-26-2009 07:11
I've got a 04 sportsman 700 never broke a axle till i put some 27'' outlaws on it. now fitted with 6'' lift and 29'' outlaws and gorillas. got a 07 ranger with factory axles and 27'' mud lites never had a problem with it. it's been beat it to hell and back on the farm still kicking. just got a razr 800 have not got alot of time on it but it got lift and tires on the way. even got the first polaris i bought 95 sportsman 400 2-stroke got 27'' outlaws 4' highlifter lift and axles and it's still running used it yesterday running some crawfish traps in our duck hole. so not a lot of complaints here. I've seen your big boy play toy in some pic's you have on here hope you were not trying the same holes as that beast. Have you ever been to the ride in alto texas want to say i've seen that truck there.