Kix,
To my knowledge tempered is usually just written as "T" as in "Q & T"
Taking a wild guess here, but could TPPO mean: Type Per Purchase Order?
A572 has 4 or 5 different types, depending on the Columbium or Vanadium content.
It is a fine grain steel.
3.2