By nitrorocket1
Date 04-27-2009 23:58
Edited 04-28-2009 00:05
I have seen the weld symbol, but my main question is;
If I start my 2" skip weld at the begining edge of the plate, do I put the fillet on the opposite side of the t-joint starting 2" in from the edge? Or do I center the 2" skip weld exactly between the skip welded 5" centers(I would have to start the fillet 2.5" from edge of plate on opposite side of the plate)??