- - By jsdwelder (***) Date 05-20-2009 12:01
I have to write a WPS for hardfacing with L605 on to 304 in accordance with ASME IX. Does anyone know what the F number and the A number would be for these?  Any help is welcomed. Thank You
Parent - - By js55 (*****) Date 05-20-2009 12:46
Do you have a copy of ASME Section IX?
Do you have a chemistry for your filler metal?
What process are you using?
Parent - By jsdwelder (***) Date 05-20-2009 13:14
Sorry, I guess my question was a bit vague. We are using GTAW and yes I do have a copy of IX.
Chemical content of wire is:
C-0.110
Mn-1.53
Si-0.19
P-0.014
S-0/.002
Cr-20.10
Ni-10.60
W-14.60
Fe-2.60
C0-BAL