I have to write a WPS for hardfacing with L605 on to 304 in accordance with ASME IX. Does anyone know what the F number and the A number would be for these? Any help is welcomed. Thank You
Sorry, I guess my question was a bit vague. We are using GTAW and yes I do have a copy of IX. Chemical content of wire is: C-0.110 Mn-1.53 Si-0.19 P-0.014 S-0/.002 Cr-20.10 Ni-10.60 W-14.60 Fe-2.60 C0-BAL