It is an innovative pipe welding solutions as a flux-cored TIG rod for the most efficient welding. MAGNA 39FC helps welders in eliminating the need for back shielding or purging using inertgas, excessive downtime, and all related set-up costs in maintenance pipe welding. The backside of the root pass can be shielded by MAGNA 39 againest the destructive impact of atmospheric gases . MAGNA 39 is an ideal in-situ maintenance welding formulation suitable applications in refineries, power station, chemical plants,or fertilizer plants. Classification : ASME/AWS A5.22 R316L T1-5