Well I guess that im hung up on the test report from the test facility that my suppier used.(I did audit the test facility and they are qualified/on my list too)
The test facility referenced my Purchase order on the report given to my supplier who in turn furnished me with it, but they referenced ASME sec III subsection NC class 2 sa-479
My Po has ASME sec III Subsection NB class 1 sa-182
So my gut tells me , or leads me to feel that it has not been tested to my requirements.
I could be wrong and tomorrow is my deadline before I send it to my Consultant ( this is our mock up ).
I’m also not sure I see all the processing data From sa479 to sa182
Seems to me that it went from being cl2 479 at testing to being 182 on the last two C of Cs.
Nothing says its been tested to what is on my po.
My plan is to list all these concerns and fax over the certs let him review, and comment on my concerns.
If any1 has experience with Nuc cert traceability and would like to see them and comment let me know.( it will take them a few days to reply always does)
Any info would be helpful.
MDK