its welding rod. 6010 5p there is also 5p+
Doesn't 5P stand for 5 plus? 6010 +++++ ?
5Ps are red rods and the 5P+ are grey
One of Lincoln Electrick's E6010 rods is named Fleetweld 5P. They are talking about this rod.
now would be a fun time to start a joke that 5P is a new joint position, and all the real dogs are certed for 5p welding
5P+ A great rod on roots,uphill or downhill.
k. thank you all. Lincoln 6010.
By Blaster
Date 11-20-2009 20:37
Edited 11-20-2009 21:32
5P is Lincoln's red 6010.
5P+ is the grey electrode you used on the 3 2G 8" schedule 80 pipe assignments you did in your first quarter. ; )