Up Topic Welding Industry / General Welding Discussion / 5P?? what is it
- - By weldstudent (**) Date 11-18-2009 02:42
[deleted]
Parent - - By Marsh Welding (**) Date 11-18-2009 02:57
its welding rod. 6010 5p there is also 5p+
Parent - - By sled_king (*) Date 11-18-2009 04:12
Doesn't 5P stand for 5 plus? 6010 +++++ ?
Parent - By jrod (**) Date 11-18-2009 05:06
5Ps are red rods and the 5P+ are grey
Parent - By DaveBoyer (*****) Date 11-18-2009 05:25
One of Lincoln Electrick's E6010 rods is named Fleetweld 5P. They are talking about this rod.
Parent - - By Metarinka (****) Date 11-18-2009 14:53
now would be a fun time to start a joke that 5P is a new joint position, and all the real dogs are certed for 5p welding
Parent - By up-ten (***) Date 11-19-2009 00:36
5P+  A great rod on roots,uphill or downhill.
Parent - By weldstudent (**) Date 11-19-2009 05:13
k. thank you all. Lincoln 6010.
Parent - By Blaster (***) Date 11-20-2009 20:37 Edited 11-20-2009 21:32
5P is Lincoln's red 6010.

5P+ is the grey electrode you used on the 3 2G 8" schedule 80 pipe assignments you did in your first quarter.  ; )